Powders

Zirconia 10Dy2O3

RPM-109

Composition
ZrO2 10Dy2O3
Particle size
-125/+10 µm
Manufacturing route
Agglomeration and Sintering
Service temperature
up to 1150 °C

Dense erosion-resistant coating for turbine hot sections.