Zirconia 9.5Dy2O3-BN-Polyester
RPM-107
- Composition
- ZrO2 9.5Dy2O3 0.7BN 4.5 Polyester
- Particle size
- -180/+10 µm
- Manufacturing route
- Agglomeration, Sintering and Blending
- Service temperature
- up to 1150 °C
Abradable material for turbine hot sections. The polymer phase controls coating porosity.